It can
regulate the glaze slip viscosity,optimized rheological property and
improve the associative property of semifinished product glaze ,enhance
the strength of glazed,and regulate the glaze layer of drying
time,obtain the smooth glazed surface.
The content of ground coat and overglaze is 0.08%-0.3% generally,less in winter . put CMC in the ball mill to grind together with other glazes , or add in 3-4 hours before leaving the ball mill .
Specification as follows:
Product :Sodium Carboxymethyl Cellulose
Molecular formula :[C6H7O2(OH)2OCH2COONa]n
Appearance : White Or Cream-colored Powder
Type : Ceramic Grade CMC TCM9
Viscosity:(2% of solution 25℃ BrooBfield L.V) 300--500
D.S : ≥ 0.92
CLˉ % : ≤1.8
PH : 6.5--8.0
Moisture % : ≤10
The content of ground coat and overglaze is 0.08%-0.3% generally,less in winter . put CMC in the ball mill to grind together with other glazes , or add in 3-4 hours before leaving the ball mill .
Specification as follows:
Product :Sodium Carboxymethyl Cellulose
Molecular formula :[C6H7O2(OH)2OCH2COONa]n
Appearance : White Or Cream-colored Powder
Type : Ceramic Grade CMC TCM9
Viscosity:(2% of solution 25℃ BrooBfield L.V) 300--500
D.S : ≥ 0.92
CLˉ % : ≤1.8
PH : 6.5--8.0
Moisture % : ≤10